#banner { position: relative; width: 1003px; height: 200px; overflow: hidden; margin: 0 auto; } #banner_list img { border: 0px; } #banner_bg { position: absolute; bottom: 0; background-color: #000; height: 30px; filter: Alpha(Opacity=30); opacity: 0.3; z-index: 1000; cursor: pointer; width: 1003px; } #banner_info { position: absolute; bottom: 0; left: 5px; height: 22px; color: #fff; z-index: 1001; cursor: pointer } #banner_text { position: absolute; width: 120px; z-index: 1002; right: 3px; bottom: 3px; } #banner ul { position: absolute; list-style-type: none; filter: Alpha(Opacity=80); opacity: 0.8; z-index: 1002; margin: 0; padding: 0; bottom: 3px; right: 20px; } #banner ul li { padding: 0px 3px; float: left; display: block; border: #e5eaff 1px solid; background: #f8fafa; cursor: pointer; font-size: 12px; } #banner ul li.on { background: #dfdfdf } #banner_list a { position: absolute; }
当前位置:首页 >新闻中心 > 不鏽鋼無縫管酸洗鈍化的過程與步驟

不鏽鋼無縫管酸洗鈍化的過程與步驟

2020-09-23 00:40   评论:07 点击:280

不鏽鋼無縫管酸洗鈍 化的過程與步驟。

1、準備工作: 2、化學除油: (1)、 化學除油采用槽內浸泡方式,除油槽用鋼板製造,內壁鋪PVC或聚乙烯。 (2)、 運用12~15%的硝酸(按體積)停止化學除油處置,溫度為40℃~60℃,時間為2~4小時。 (3)、不鏽鋼無縫管在槽內浸泡時,應留意放置的位置,防止管內存留空氣。 (4) 、 浸泡過程中應上下前後挪動或翻動不鏽鋼無縫管,使內腔溶液不時改換,以進步效果。必要時取出不鏽鋼無縫管,用 水氣衝洗後再停止浸泡。 (5) 、 化學除油直至不鏽鋼無縫管外表完整被水潤濕。 3、熱水漂洗: (1)、除油後的不鏽鋼無縫管從除油槽內取出,浸泡在40℃~60℃左右的熱水槽內漂洗,時間5~20分鍾。 (2)、熱水槽用鋼板製造,內壁鋪PVC或聚乙烯。 (3)、水中氯離子含量小於25ppm。 4、用水衝洗: (1)、水漂洗過的不鏽鋼無縫管用壓力水(壓力P≥0.1Mpa)停止衝洗。 (2) 、水中氯離子含量小於25ppm。 5、鈍化: (1)、鈍化采用池內槽泡方式,鈍化液配方和浸泡時間依照2.3表任選一種。 (2)、鈍化槽鋼板製造,內壁鋪防酸塑料。 (3)、槽內浸泡時,應留意放置的位置,防止不鏽鋼焊管內存留空氣。 (4)、浸泡過程中應上下前後挪動或翻動不鏽鋼無縫管,使內腔溶液不時改換,以進步效果。必要時取出不鏽鋼無縫管,用水 氣衝洗後再停止浸泡。 6 、枯燥: 經過鈍化的不鏽鋼無縫管,要抓緊用幹淨的緊縮空氣或氮氣吹幹,並且必需有足夠的時間(至少2小時)使不鏽鋼無縫管 在空氣中自然鈍化。 7、檢驗: 不鏽鋼無縫管經鈍化後,應停止自檢、互檢,然後提交質檢員按請求停止驗收 。 8 、維護: (1)、如外外表需求停止油漆的不鏽鋼無縫管,則依照塗裝請求停止。 (2)、檢驗合格後的不鏽鋼無縫管,不鏽鋼無縫管廠家要用塑料塞封口,用三防布停止包紮維護,並停止標識。

上一篇:32*4汽車半軸套管標準 32*4承壓設備用無縫鋼管 32*4汽車半軸用無縫管化學成分
下一篇:不鏽鋼管價格還將承接年前的弱勢 ,負重前行

我来说两句已有07条评论,点击全部查看
我的态度:

网站首页| 公司概况| 荣誉资质| 产品展示| 销售网络| 公司团队| 公司新闻| 钢管知识| 联系我们| 网站地图